My Customer Says the Candle Tunnels but My Retained Sample Burns Perfectly — Is It the Wick or the Way They Burned It?
शेयर करना
So was it the customer's fault? Not established — and do not say it, even privately. That is a conclusion, not a finding, and a maker who reaches it by default stops learning from complaints. The honest answer here is not yet known.
How do I find out? Burn retained samples twice over — one set the way you always burn them, one set the way the customer described. Three outcomes, each pointing somewhere different. Protocol here.
Is there a CSI wick chart to look up instead? No. CSI publishes no jar-diameter recommendation and no wick sizing chart of any kind — the range is described by thickness words only. Your own burn record is the only authority, and do not accept a sizing claim from any supplier, ours included, without the test conditions behind it.
- The straight answer
- What the retained sample proves — and what it does not
- Why an adequately wicked candle still tunnels
- The five questions, and how to word them
- The two-arm reproduction test
- Retained samples, traceability and the two free checks
- What the test costs against what re-pouring costs
- FAQ
What the retained sample proves — and what it does not
Be exact about the claim your sample supports. You lit a jar from the same batch, it reached the glass, the surface stayed level, and you concluded the batch is sound. What you demonstrated is narrower: this formula, in this vessel, with this wick, is capable of a full melt pool under your burn conditions. Capability — not compliance, not uniformity, and nothing about the room the complaint came from.
Three ordinary gaps sit between your jar and theirs. The unit is not the same unit: a pour run is not homogeneous — first jar and last jar come off the pitcher at different temperatures, a wick can sit a millimetre off centre on one unit and not another, a sticker can lift. The jar is not necessarily the same jar: glass arrives in cartons from different production runs, so unless you measure each one, "the same jar" means "the same SKU". And the burn is definitely not the same burn: yours happened in your workspace, at a length you chose, wick trimmed by reflex. Theirs happened somewhere you have never been.
The symmetry runs both ways. A maker who always burns three or four hours at a stretch will find that an under-wicked candle looks perfectly acceptable, because a long session has time to widen the pool to the wall even from a slow start. Your generosity as a test burner can hide the exact fault you are trying to rule out — which is why the test below has two arms.
Why an adequately wicked candle still tunnels in someone else's room
Tunnelling is not an event, it is a path a candle gets locked onto. The mechanism is worth knowing properly, because it lets you reason about the customer's answers rather than guess.
Two things follow. A candle can be adequately wicked and still tunnel in use, if nobody gives the first session time to reach the wall. And a candle can be under-wicked and still look faultless to its maker, if the maker always burns long. Those are one fact seen from two ends, and together they are why a single perfect retained sample cannot settle a tunnelling complaint.
The five questions, and how to word them
Every one of these can be heard as an accusation, and a customer who feels accused stops describing and starts defending. Two framings fix most of it. Put the burden on your product, not their behaviour — you are gathering information, not building a case. And offer the replacement before you ask anything, so the questions are clearly not a test they must pass to get one. That reordering improves the answers more than any phrasing trick.
| # | Ask, in these words | What the answer changes |
|---|---|---|
| 1 | "Roughly how long do you usually leave it burning in one sitting — half an hour, an hour, an evening?" | The most informative number on the list, offered as a menu so no answer feels wrong. It sets the session length for Arm B of the test |
| 2 | "About how many times has it been lit so far?" | Separates "narrow from the first burn" from "narrowed gradually". Two burns and a deep well is a different story from ten |
| 3 | "Do you trim the wick before lighting? Some people do, plenty don't — either is useful for me to know." | Sets Arm B's trimming condition, with permission to say no built into the question. Also explains a mushroomed or recessed flame in the photo |
| 4 | "Where does it usually sit when it's lit — a table, a shelf, a windowsill, a bathroom?" | Position, and by implication room size and draught exposure. A windowsill or corridor shelf points straight at airflow; a small closed room points away from it |
| 5 | "Was a fan or the AC running while it burned? I ask because moving air pulls the flame to one side." | Airflow, with the mechanism stated so the question reads as technical rather than accusatory. A yes makes a lopsided pool the leading explanation and adds airflow to Arm B |
| 6 | "Could you send two photos — one straight down from above with it lit, and one of the surface when it's completely cold and set?" | The physical evidence, and the reason to specify straight down. A narrow concentric pool, a lopsided pool and a recessed flame in a deep well are three different diagnoses |
Read the two photographs together. The lit overhead shot shows where the flame sits relative to centre, whether the pool is round or crescent-shaped, and whether the flame is down inside a well. The cold shot shows the finished geometry without the flame in the way: the width of the unmelted ring, whether it is even all round, and whether the surface is level or cratered. A narrow concentric column with an even ring reads as a short-session history; a crescent pool reads as airflow; a deep narrow well after two or three lightings is the pattern that should make you take the wick question seriously.
The two-arm reproduction test
The design principle is one sentence: burn the candle their way, not your way. Every maker's instinct is to relight a retained sample and watch it behave — which reproduces the maker's conditions and therefore the maker's result. What you do not know is what it does in forty-minute stretches on a windowsill with the fan on.
Take six retained jars from the complained-of batch, eight if you have them, and split them into two arms of three. Hold the batch and the wick constant — same pour, same wick lot, same jar SKU — and change only the burn pattern. Vary the wick too and you have destroyed the experiment before lighting it: two variables moving together tell you nothing about either.
| Stage | Arm A — your usual pattern | Arm B — the customer's reported pattern | Record each session |
|---|---|---|---|
| Jars | 3 retained jars, same batch and wick lot | 3 retained jars, same batch and wick lot | Jar number, batch code, pour date, position in the pour run |
| Session length | Your habitual test length, whatever it actually is | The length they reported, to the nearest ten minutes | Start and stop time by the clock, not by estimate |
| Trimming | Trimmed as you always trim | Matched to what they said — including not at all | Whether trimmed, and roughly to what length |
| Airflow | Still air, door closed | Fan or AC running if they mentioned one | Fan or AC on/off, and roughly where it pointed |
| Sessions | As many burns as the customer reported | The same number as Arm A, so the comparison is fair | Minutes from lighting until the pool touches the glass — or that it never did |
| Measure & photograph | Weigh cold before and after; shoot straight down, lit | Weigh cold before and after; shoot straight down, lit | Mass in grams, room temperature, plus a cold-surface photo once set |
Weighing matters more than it looks. A cold mass before and after every session, on a ₹354 weighing scale, turns an argument about appearance into numbers you can compare between arms — and it survives you forgetting what the jar looked like three weeks later.
| Outcome | What it establishes | What it does not | Your next move |
|---|---|---|---|
| Arm B tunnels, Arm A does not | The reported usage is sufficient on its own to produce the complaint — a complete causal explanation that needs no defect | That the wick is ideal. Sufficient is not the same as sole | Send the replacement with a first-burn instruction, not a rebuttal. Then ask honestly whether that burn pattern is common among your customers — if it is, re-wicking is a product decision, not an admission |
| Both arms tunnel | The wick is implicated: the candle does not reliably open to the glass even under your own favourable pattern | Which wick to use instead, or by how much it is off. That has to be tested, not looked up | Run a deliberate single-variable trial on a small fresh pour — wick thickness only, wax, load and jar fixed. Quarantine the rest of that batch while you do |
| Neither arm tunnels | The formula, wick and jar combination behaves under both patterns. The problem is specific to that unit or that piece of glass | That the customer is mistaken. An off-centre wick or an odd jar is a real fault with a real cause | Inspect the individual unit: wick centring, sticker adhesion, the internal profile of that jar, its position in the pour run. Then look at pour-line consistency, not your recipe |
Retained samples, traceability and the two free checks
All of the above assumes you kept samples. If you did not, the first corrective action from this complaint is not a wick change — it is starting to keep them, from the next batch you pour. Without them a complaint is one person's memory against your own, and no reasoning closes that gap.
A batch code is only as good as what it connects to. If your records turn it into nothing but a date, you cannot investigate — only guess more confidently. A batch number must resolve internally to all nine of these.
| Field | Record | Why a complaint needs it |
|---|---|---|
| Wax lot | Product, pack size, invoice date and number | Shows whether complaints cluster on one lot rather than on your method |
| Fragrance lot | Oil, size, invoice date and number | Same logic, and lets you check the load against the wax's published ceiling |
| Wick lot | Type and thickness as the listing describes it, pack size, invoice date | Without it, "we changed wicks in March" is folklore rather than a testable fact |
| Jar shipment | Product, pack size, invoice date, and the carton if you split across cartons | An odd internal profile in one carton is invisible unless the carton is recorded |
| Pour date | Date, plus the time the run started and finished | Sets cure age at the point of sale and at the point of complaint |
| Fragrance-add temperature | The reading on the thermometer, not the target | One of the two free checks below. A cold add is a real and common cause |
| Pour temperature | The reading at the moment of pouring | Drives adhesion, surface finish and how the column sets |
| Load | Percentage and the actual grams weighed | 15 g in a 150 g candle is 10% — write both so the arithmetic is auditable |
| Position in the run | Which third of the run each unit came from | The field most makers skip, and the one that finds intermittent faults |
Now the two checks that cost nothing and should come before you spend a rupee: both are documented constraints and both produce burn complaints.
What the test costs, against what re-pouring costs
The case for gathering evidence is arithmetic. Figures are CSI live pricing, September 2026, on a 150 g soy container candle at a 10% load — 135 g wax, 15 g oil — in a jar that publishes its fill capacity, which most jar families do not. Where a jar publishes none, pour one and weigh it: "200 ml" is a volume, not a 200 g fill, and a 200 ml salsa jar at ₹29.50 each in packs of 50 or 100 takes whatever mass it takes.
| Line | Rate used | 8 test candles | 300-candle re-pour |
|---|---|---|---|
| Wax — CSI 464 flakes, 135 g per candle | ₹507.40 / kg | 1.08 kg = ₹548.00 | 40.5 kg = ₹20,549.70 |
| Fragrance — British Rose, 15 g per candle | ₹3,068 / kg = ₹3.068 / g | 120 g = ₹368.16 | 4.5 kg = ₹13,806.00 |
| Glass — Clear Glass Jar with Golden Lid, 150 g | ₹944 / pack of 10 = ₹94.40 each | 8 jars = ₹755.20 | 300 jars = ₹28,320.00 |
| Wick — Eco Candle Wicks, Thin (C1) | ₹5.90 each at every pack size | 8 wicks = ₹47.20 | — |
| Wick — Eco Candle Wicks, Thick (C2) | ₹188.80 / 20 · ₹4,720 / 500 = ₹9.44 each | — | 300 wicks = ₹2,832.00 |
| Wick stickers | ₹100 / sheet of 40 = ₹2.50 each | 8 = ₹20.00 | 300 = ₹750.00 |
| Care stickers | ₹413 / 500 one-inch = ₹0.83 each | — (not shipped) | 300 = ₹249.00 |
| Total, glass included | — | ₹1,738.56 · ₹217.32 per candle | ₹66,506.70 |
| Total if the glass is recovered and reused | — | — | ₹38,186.70 |
So the test costs about 4.6% of a re-pour that reuses the glass, and about 2.6% of one that does not — and that is the expensive version, where you keep no retained samples and must pour a set specially. If you already keep retained samples it costs ₹0 in materials and about a week of evenings. Against a decision that could commit ₹38,186.70 of stock to the bin, there is no version of this arithmetic in which guessing wins.
| Size | Price | Per kg | 135 g pours |
|---|---|---|---|
| 500 g | ₹260.00 | ₹520.00 | 3 |
| 1 kg | ₹507.40 | ₹507.40 | 7 |
| 5 kg | ₹2,537.00 | ₹507.40 | 37 |
| 10 kg | ₹5,074.00 | ₹507.40 | 74 |
| Pack | Thin (C1) | Thick (C2) | Per wick |
|---|---|---|---|
| 10 wicks | ₹59.00 | out of stock | C1 ₹5.90 |
| 20 wicks | ₹118.00 | ₹188.80 | ₹5.90 / ₹9.44 |
| 50 wicks | ₹295.00 | ₹472.00 | ₹5.90 / ₹9.44 |
| 100 wicks | ₹590.00 | ₹944.00 | ₹5.90 / ₹9.44 |
| 500 wicks | ₹2,950.00 | ₹4,720.00 | ₹5.90 / ₹9.44 |
Now the part against our own interest, because it is true. The most likely outcome of this investigation is that you buy nothing. Most single tunnelling complaints resolve into a short first burn, a draughty position, or a jar from the tail of a pour run, and none of those is fixed by a purchase order. We would rather sell you one roll of care stickers at ₹413 and keep you for five years than sell you 500 wicks you did not need.
CANDLEMAKINGSUPPLIESINDIA supplies raw materials, not finished candles. The commercially convenient version of this page would tell you your wick is undersized and link you to a bigger one. We sell wicks. We are not doing that, because we publish no sizing data that could justify it, and because a maker who re-wicks a sound formula on one complaint gets worse candles — and then stops reordering.
What we do not publish, said once and clearly: no jar-diameter recommendation, no burn-diameter figure, no melt-pool width, no burn rate, no flame height and no wick sizing chart, for any wick in the range. Eco Candle Wicks are listed as Thin (C1) and Thick (C2), and that is the whole published specification. Nothing here assigns a wick to a jar width.
Every price is taken from live CSI stock in September 2026 and links to the product page, where current pricing, stock and specification take precedence. The 13%, 10% and 13% fragrance ceilings belong to Luxury Soy Wax Chunks, Luxury Soy Wax CSI 464 and Premium Coconut Soy CSI 468 respectively; they are wax-manufacturer formulation limits, not regulatory limits, and the other thirteen waxes publish none. Burn-safety guidance on your own label, and any decision to release or withdraw a batch, are yours and carry your liability, not ours. For bulk pricing, GST invoicing, MSDS and IFRA documentation, message us on WhatsApp at +91 7397976926.
Frequently asked questions
- Best wick for candle making — the general guide by diameter (principles, not a CSI specification)
- How to verify wax quality before you buy in India
- The complete candle making raw material list
- How to price candles in India in 2026
- Is candle making actually profitable in India in 2026?
- Scaling to 1,000 orders a month
Customer reviews: The six reviews at the top are genuine, published Judge.me reviews left on CSI product pages — two on Luxury Soy Wax CSI 464, one each on Premium Coconut Soy CSI 468, Luxury Soy Wax Chunks, Clear Glass Jar with Golden Lid and Gardenia Fragrance Oil. All six are recorded by Judge.me as verified buyers. Names, ratings, dates and products are as recorded; one longer review is shortened with an ellipsis and otherwise unedited. None of them describes tunnelling, a melt pool, wick performance or a customer complaint about a finished candle, and none is offered as evidence about burn behaviour.
What is deliberately absent: no wick is matched to a jar diameter, and no melt-pool width, burn-diameter figure, burn rate, flame height or consumption rate appears anywhere above, because CSI publishes no wick sizing data of any kind — the range is described by thickness words only (Eco Candle Wicks in Thin (C1) and Thick (C2), plus Cotton Braided Ready Made, Performance Wooden Wicks and braided wick by the metre). No safety verdict, maximum burn time or glass-temperature limit is given, because none is published and burn guidance is the brand owner's responsibility.
Figures verified September 2026 (CSI live pricing): Fragrance ceilings are the wax manufacturers' stated maximum loads — 13% Luxury Soy Wax Chunks, 10% Luxury Soy Wax CSI 464, 13% Premium Coconut Soy CSI 468 — formulation limits, not regulatory limits; the other thirteen waxes publish none. Listing temperatures cited as instructions: Eco Soy CSI 400 fragrance addition at 85°C (185°F) within 80–90°C; CSI 464 melt and pour 80–90°C; CSI 468 pour 58–60°C; Luxury Soy Chunks 75–80°C (the overlap of two figures on the same listing). CSI 464 and CSI 468 both state a 60-month shelf life in cool, dry storage. All cost arithmetic assumes a 150 g candle at a 10% load (135 g wax, 15 g oil): Luxury Soy CSI 464 ₹507.40/kg (500 g ₹260, 1 kg ₹507.40, 5 kg ₹2,537, 10 kg ₹5,074); British Rose Fragrance Oil ₹3,068/kg = ₹3.068/g; Clear Glass Jar with Golden Lid 150 g ₹944 per 10 = ₹94.40 each; Eco Candle Wicks Thin (C1) ₹5.90 each and Thick (C2) ₹9.44 each (C2 pack of 10 out of stock; 20 wicks ₹188.80, 50 ₹472, 100 ₹944, 500 ₹4,720; C1 10 ₹59, 20 ₹118, 50 ₹295, 100 ₹590, 500 ₹2,950); Candle Wick Stickers ₹100 per sheet of 40 = ₹2.50 each; Candle Care Stickers Roll ₹413 per 500 one-inch = ₹0.83 each. Eight test candles: ₹548.00 wax + ₹368.16 oil + ₹755.20 glass + ₹47.20 wicks + ₹20.00 wick stickers = ₹1,738.56 (₹217.32 each). A 300-candle re-pour on Thick (C2): ₹20,549.70 wax + ₹13,806.00 oil + ₹2,832.00 wicks + ₹750.00 wick stickers + ₹249.00 care stickers = ₹38,186.70 with the glass recovered, or ₹66,506.70 including 300 fresh jars at ₹28,320.00. One shippable replacement: ₹68.50 + ₹46.02 + ₹94.40 + ₹5.90 + ₹2.50 + ₹0.83 = ₹218.15. Also cited: Luxury Soy Chunks from ₹299/500 g, Premium Coconut Soy CSI 468 from ₹325/500 g, Eco Soy CSI 400 ₹399/kg, cheapest wax Semi Refined Paraffin ₹220/kg, 200 ml Salsa Glass Jar ₹200.60 per 5 and ₹2,950 per 100 (₹29.50 each), Cotton Braided Wicks Ready Made ₹120 per 10, Performance Wooden Wicks ₹590 per 10, Wick Centering Device ₹118 per 5, Pen Thermometer ₹354, Candle Making Weighing Scale ₹354, Candle Wick Cutter / Trimmer ₹295, and 92 fragrance oils live in the Fragrance Oils collection. Most jar families publish no fill capacity — pour one and weigh it; "200 ml" is a volume, not a 200 g fill. Prices, stock and specifications change — the linked product pages are always authoritative.